Your present location:Home > Products > Engineering Steel

BS EN34/665M17 | ASTM 4615/4617 Engineering Steel

Port: Hu nan

engineering steel, cold work tool steel, hot work tool steel, plastic mold steel, spring steel, high speed steel, stainless steel

Alloy Structural Steel, Alloy Tool Steel, Carbon Structural Steel, Carbon Tool Steel, Bearing Steel, Spring Steel ,Stainless Steel, Refractory Steel, Roll Steel, Pinion Steel. Additionally, the company also has the capacity to forge round steel, steel flat, square steel, module, shaft and roller

E-mail:export@qilucs.com

  • Quick Details

    1: AISI EN34 steel introduction
        EN34 is a 2% nickel, molybdenum case hardening steel grade. Combining good core strength, toughness and fatigue resistance this grade can be case hardened up to 60HRc. EN34 is suitable for applications requiring wear resistance and shock resistance. It offers good core strength and impact properties with little temper brittleness.
     
    2: AISI EN34 Steel equivalent
    Country China Japan Germany USA British
    Standard GB/T 3077 JIS G4105 DIN (W-Nr.)
    EN 10250
    AISI/ASTM
    ASTM A29
    BS 970
    Grade / / / 4615/4617
    EN34/665M17
     
    3: AISI EN34 steel chemical composition
    Grade C Si Mn P S Mo Ni
    EN34/665M17 0.14-0.20 0.10-0.35 0.35-0.75
    0.035 max 0.040 max 0.20-0.30 1.50-2.00
    4615/4617 0.13-0.18 0.15-0.30
    0.45-0.65
    0.035 max 0.040 max 0.20-0.30 1.65 -2.00
     
    4: AISI EN34 steel mechanical properties
        The mechanical properties mainly include tensile strength, yield strength, elongation, area or reduction, hardness, impact value, non-metalic inclusion etc. Different heat treatment, the mechanical properties will be different, such as normalized, tempered, QT. If you want to know the properties, kindly contact the salesman.
      
    5: AISI EN34 steel overviews

    Size Round Dia 6-1200mm
    Plate/Flat/Block Thickness
    6mm-500mm
    Width
    20mm-1000mm
    Heat treatment Normalized ; Annealed ; Quenched ; Tempered
    Surface condition Black; Peeled; Polished; Machined; Grinded; Turned; Milled
    Delivery condition Forged; Hot rolled; Cold drawn
    Test Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc. 
    Payment terms T/T;L/C;/Money gram/ Paypal
    Trade terms FOB; CIF; C&F; etc..
    Delivery time 30-45 days
    Application AISI EN34 is suitable for shafts, gears, transmission parts, camshafts and cams, cam shafts connecting rods crankshafts gears.

    7. Carburising / Case Hardening
        Carburising and case hardening will give a hard wear resisting surface and a tough core strength to the steel. EN34 is suited for carburising and case hardening. Surfaces must be free from dirt and grease, and of low sulphur content. Case hardening can be carried out in salt baths with selected content depending on the type of salt and the depth of penetration required. Other considerations during the heat treatment process include the type of furnace, quenching medium and work piece transfer facilities. Time, temperatures and salt selection will be advised by your heat treatment provider.

    8. Heat Treatment
        Heat treatment temperatures, including rate of heating, cooling and soaking times will vary due to factors such as the shape and size of each EN34 steel component. Other considerations during the heat treatment process include the type of furnace, quenching medium and the work piece transfer facilities. Please consult your heat treatment provider for full guidance on heat treatment of EN34 case hardening steel.



    9: Delivery condition
        For hot forged or hot rolled bar, usually the delivery condition is hot forged or rolled, annealed, rough turned.
        For hot forged plate, usually the delivery condition is hot forged, annealed, milled surface.
        For hot rolled plate, usually the delivery condition is hot rolled, annealed, black surface.